This investigation addressed the possibility of producing pellet feed at a silica content of <= 1.0% using a representative sample of Samarco's mechanical flotation tailings. This sample contained 11.0% Fe and presented an F(80) = 116 mu m and a d(50) = 63 mu m. The higher silica content was verified in the coarser fractions and the higher iron content in the fraction. -37 mu m. Specular hematite is the most abundant mineralogical phase in the fraction -37 mu m. The technological tests used one of four methods: magnetic concentration using a wet high-intensity magnetic separator, magnetic concentration using a S Lon high-gradient magnetic separator, reverse flotation or direct flotation. The methods using the magnetic concentrator SLon, reverse flotation and direct flotation did not present results meeting the target of the study: iron content in the concentrate (rougher stage) greater than 34% or iron recovery greater than 80%. Cleaner stages were not achievable with the resulting concentrates. In contrast, the most successful method consisted of using wet high-intensity magnetic separators (WHIMS) as a rougher stage and reverse flotation as a cleaner stage. Using this route, it was possible to produce a pellet feed with a silica grade of 1.0% and high specular hematite content.

  • 出版日期2010-8