摘要

Morphological and spectroscopic studies of Sr2CeO4 blue phosphor in the form of fine particles prepared from a powdered multicomponent precursor, via a combustion method, are reported. Samples were also prepared through a solid-state reaction and from a polymeric precursor for comparison. Citric acid or glycine as fuels in the combustion method lead to a mixture which is heated at 950 degreesC for 4 h, resulting in spheroidal particles with a diameter between 250-550 rim. Samples from the polymeric precursor result in spheroidal particles (350-550 nm) and from the solid-state reaction in irregular particles (similar to5 mum). Therefore, the combustion method is adequate for preparation of Sr2CeO4 in the form of spherical fine particles.