摘要
Experiments demonstrated that the addition of a minute amount of V to Fe52Co(20-x)B20Si4Nb4Vx amorphous alloy induces atomic-scale phase separation, which dramatically enhances the plasticity. Especially, Fe52Co17.5B20Si4Nb4V2.5 amorphous alloy exhibited a strength of 4.7 GPa and a fracture strain of 8.0%, which is the largest strain reported for Fe-based amorphous alloys. In this study, the structural origin of the enhanced plasticity is explored by examining the role played by the phase separating element on the packing density and strain localization.
- 出版日期2012-8-30