In this study, a novel method was used to synthesize beta-TCP/HAP biphasic ceramic scaffold from natural cancellous bone. Bovine bone was calcined to remove the organic content. The remaining material was then soaked in P(2)O(5) solution for different periods. P ions were doped into cancellous bone and reacted with hydroxyapatite (HAP) to produce beta-tricalcium phosphate (beta-TCP) at room temperature without any subsequent high-temperature heat treatment. By increasing the soaking time, the crystalline phase composition of the calcined bone gradually changed from HAP into a HAP/beta-TCP biphasic structure with different HAP/TCP ratios. The crystallite size of HAP and beta-TCP was smaller than 100 nm.