FAU-*BEA-types zeolites pellets were elaborated with a hydraulic press in the presence of a small amount (5 wt%) of binder [methylcellulose (MC) or anhydrous sodium metasilicate (Na2SiO3)] for molecular decontamination, in particular for the space field. Nitrogen sorption-desorption revealed a small loss of micropore volume (10%) with a compression load of 6 tons (0.24 cm(3)/g instead of 0.27 cm(3)/g for the mixture of FAU and *BEA-types zeolites powders), which can be attributed to a partial amorphization. Adsorption kinetics of n-hexane, and cyclohexane showed that the optimum pellets can adsorb volatile organic compounds. For example, FAU-*BEA-type zeolite powder mixture (50 wt% of each zeolite) adsorb 130 mg of n-hexane per g of anhydrous zeolite whereas the pellets made with 5 wt% of MC or Na2SiO3 adsorb about 117-118 mg of n-hexane per g of anhydrous zeolite. These results are coherent with the ones obtained with the cyclohexane and nitrogen adsorption where a small loss of the adsorption capacities was observed.