摘要

A transparent triaxial cell was designed and manufactured using acrylic resin. The cell was used to conduct strength and creep tests. Photographs were taken of the specimens at constant time intervals during the constant strain rate test. Photographs were also taken at constant intervals of strain during the creep test, but this rate was changed to one image per second when the specimens first showed tertiary creep. Comparison of the axial and lateral strains during the constant strain-rate and creep tests indicated no significant differences between the two tests. It is well known that the axial creep strain rate is inversely proportional to remaining life in tertiary creep. This study showed that the lateral creep strain rate is also inversely proportional to remaining life. The constant strain-rate tests were conducted with transparent end pieces attached firmly to the upper and lower ends of the specimens. Three holes were drilled into the end pieces, and water was expelled into the holes when the specimens were compressed. It was clearly observed that the water began. owing from the holes back into the specimen during the volumetric expansion of the specimen. The transparent triaxial cell permitted easy observation of water ejection and re-absorption into the specimens.

  • 出版日期2008-3