摘要

A bath of electroless plating Ni on the AZ91D magnesium alloy, containing sulfate nickel, was given in this paper. The nucleation mechanism of Ni-P deposits on the AZ91D magnesium alloy was studied by XRD and SEM. The electroless Ni-P deposits were preferentially nucleated on the β(Mg17Al12) phase and extended to the primary and eutectic αphases of the AZ91D magnesium alloy.