Limits of the CIL circuit in copper-gold plants

作者:Burns Fraser*; Peng Yongjun; Seaman David; Bradshaw Dee
来源:Minerals Engineering, 2014, 55: 132-137.
DOI:10.1016/j.mineng.2013.10.008

摘要

This study examined the performance of the CIL (Carbon-in-Leach) circuit at Telfer, a copper-gold plant treating porphyry copper deposits containing gold associated with both copper and iron sulphides, with an objective to identify factors normally limiting the gold recovery in the CIL circuit in the presence of a small amount of copper after copper flotation, and then propose a means to improve it. Diagnostic leaching assessment and mineralogical analysis by MLA revealed that the occlusion of gold by other minerals and the fine grain size of gold associated with them may be the contributing factors to the low gold recovery in the CIL circuit. Fine grinding of the CIL feed increased gold recovery significantly from the leaching process. However, it is interesting to find that fine grinding increased the amount of released copper ions which complex with cyanide resulting in significantly higher cyanide consumption. It is therefore proposed that regrinding of the CIL feed followed by copper flotation is an appropriate pre-treatment method for the CIL circuit.

  • 出版日期2014-1